Hydrogen Embrittlement of SS316L Instrument Tubing in a Hydroprocessing Unit

An unexpected failure of 316L Stainless Steel instrument tubing occurred in a high pressure Hydroprocessing unit resulting in a shutdown of the unit. The tubing system consisted of a compression type fitting commonly used in instrument systems and had only been in service for 3 years when the failure occurred. The failed tubing samples were removed for metallurgical analysis and determination of damage mechanism.   

Metallurgical analysis and finite element analysis of the tubing identified excessive cold working leading to hydrogen embrittlement as the primary mode of failure. This paper details the investigation into the failure to arrive at the root cause and the preventive measures adopted to assess the installed population of tubing in similar service.  

 

Product Number: 51320-14357-SG
Author: Siew Leong Waia, Rajaram Chidambaramb, John Richertc, Jorge Perdomo
Publication Date: 2020
$0.00
$20.00
$20.00
Also Purchased
Picture for 05098 A Review on Hydrogen Embrittlement of
Available for download

05098 A Review on Hydrogen Embrittlement of Duplex Stainless Steels

Product Number: 51300-05098-SG
ISBN: 05098 2005 CP
Author: Thierry Cassagne and Freddy Busschaert, Total France
$20.00
Picture for 08407 Hydrogen Permeation of Alloy 22
Available for download

08407 Hydrogen Permeation of Alloy 22

Product Number: 51300-08407-SG
ISBN: 08407 2008 CP
Author: Matthew Taylor and Leslie McMillion
Publication Date: 2008
$20.00