Aluminization of Ni-Base Superalloys by Slurry and Pack Cementation Processes

Aluminide coatings were produced by halide activated pack cementation (HAPC) and halide activated slurry cementation (HASC) on Ni-base superalloys (UNS N07208 UNS N06230 and UNS N07718). Both HAPC and HASC are in situ chemical vapor deposition processes activated by halide salts. The chemical reactions deposit the desired element (aluminum in this case) on the surface of metallic alloys. The coating element subsequently diffuses into the substrate to modify the surface of the underlying alloy. Under oxidizing conditions the surface modified alloy forms a passive oxide layer that protects it from high temperature corrosion. In this study the characteristics of coatings applied by the pack and slurry cementation processes i.e. thickness microhardness microstructure and elemental distribution were studied using a broad range of techniques - X-ray diffraction (XRD) macrophotography optical and scanning electron microscopy with energy dispersive spectroscopy (SEM/EDS). The HAPC and HASC processes resulted in different coating characteristics. The HAPC process produced more consistent coating microstructures and thicknesses while the coatings applied by the HASC process were more variable. The effectiveness of HAPC and HASC coatings in high temperature environments was studied using isothermal oxidation testing.

Product Number: 51319-13487-SG
Author: Kailey Hanan
Publication Date: 2019
$0.00
$20.00
$20.00
Also Purchased
Picture for 07209 Corrosion Behavior of Aluminized and Chromized Carbon Steel in Fluctuating Oxidizing-Sulfidizi
Available for download

07209 Corrosion Behavior of Aluminized and Chromized Carbon Steel in Fluctuating Oxidizing-Sulfidizing Environments

Product Number: 51300-07209-SG
ISBN: 07209 2007 CP
Author: Vikas R. Behrani and Preet Mohinder Singh
Publication Date: 2007
$20.00
Picture for 05418 Gas Phase Embrittlement and Time Dependent
Available for download

05418 Gas Phase Embrittlement and Time Dependent Cracking of Nickel Based Superalloys

Product Number: 51300-05418-SG
ISBN: 05418 2005 CP
Author: David Woodford, Materials Performance Analysis
$20.00
Picture for 01388 Effect of ID Surface Modification
Available for download

01388 Effect of ID Surface Modification on Carburization of Ethylene Furnace Tubes

Product Number: 51300-01388-SG
ISBN: 01388 2001 CP
Author: Arun R. Kurlekar, George T. Bayer, Gerald E. Gapinski
$20.00