06442 POSSIBLE GLYCOL CORROSION IN NOMINALLY DRY GAS PIPELINES

Pipeline quality gas is normally dried in Triethylene Glycol (TEG).  This paper explores how TEG vapor can exist in a pipeline in a similar manner to water, and possibly lead to corrosion. TEG vapor can condense at long distances down a gas pipeline as the line cools.

Product Number: 51300-06442-SG
ISBN: 06442 2006 CP
Author: John S. Smart, III, Randy Roberts
Publication Date: 2006
$0.00
$20.00
$20.00

Pipeline quality gas is normally dried in Triethylene Glycol to reduce its water dew point to below the lowest operating temperature in a pipeline, and the presence of glycol as a vapor into the gas has been regarded as insignificant. This paper explores how TEG vapor can exist in a pipeline in a similar manner to water, and possibly lead to corrosion. TEG vapor can condense at long distances down a gas pipeline as the line cools, with most condensing above 60oF. However, even the small quantities involved accumulate with volume and time, and can become significant. The corrosion rate of steel in glycol is lower than for water and the problem is a long term one. In-Line Inspection for gas pipelines should pick up internal corrosion as well as external corrosion. Lines that are “not piggable” should be rinsed with a water/methanol slug driven by a foam disc pig to reduce risk when high risk areas such as low spots under rivers are present.

Keywords: Glycol, Triethylene Glycol, glycol corrosion, dew point, gas pipeline internal corrosion

 

Pipeline quality gas is normally dried in Triethylene Glycol to reduce its water dew point to below the lowest operating temperature in a pipeline, and the presence of glycol as a vapor into the gas has been regarded as insignificant. This paper explores how TEG vapor can exist in a pipeline in a similar manner to water, and possibly lead to corrosion. TEG vapor can condense at long distances down a gas pipeline as the line cools, with most condensing above 60oF. However, even the small quantities involved accumulate with volume and time, and can become significant. The corrosion rate of steel in glycol is lower than for water and the problem is a long term one. In-Line Inspection for gas pipelines should pick up internal corrosion as well as external corrosion. Lines that are “not piggable” should be rinsed with a water/methanol slug driven by a foam disc pig to reduce risk when high risk areas such as low spots under rivers are present.

Keywords: Glycol, Triethylene Glycol, glycol corrosion, dew point, gas pipeline internal corrosion

 

PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Also Purchased
Picture for 98221 WHY DOES GLYCOL INHIBIT CO2
Available for download

98221 WHY DOES GLYCOL INHIBIT CO2 CORROSION?

Product Number: 51300-98221-SG
ISBN: 98221 1998 CP
Author: Egil Gulbrandsen, Jean-Herve Morard
$20.00
Picture for 00498 CORROSION OF CARBON STEELS IN MONOETHYLENE
Available for download

00498 CORROSION OF CARBON STEELS IN MONOETHYLENE GLYCOL

Product Number: 51300-00498-SG
ISBN: 00498 2000 CP
Author: J.J. Gonzfilez, M.E. Afonso, G. Pellegrino
$20.00