This standard practice covers the care, handling, transportation, and installation of internally plastic-coated (IPC) oilfield tubular goods and accessories (IPC material). Some internal plastic coatings are inherently brittle or may be incom- patible with various chemicals used in oil and gas production operations and therefore are susceptible to damage from poor handling procedures, well operations, and chemical attack. Coating damage (e.g., cracks, chips, and disbond- ment) reduces coating effectiveness and results in premature coating failure.