A repair of a refractory lined product gas transfer line at a hydrogen plant required welding of aged 21Cr 33Ni 1Nb castings. The repair weld procedure that was developed was the result of past experiences of industry experts as well as trial and error in the field. Subsequent to the field work, laboratory investigations were performed in an attempt to understand metallurgical issues associated with weld cracking in this alloy. Key words: liquation cracking, niobium carbides, high temperature HAZ cracking, reformer outlet, high temperature castings
A repair of a refractory lined product gas transfer line at a hydrogen plant required welding of aged 21Cr 33Ni 1Nb castings. The repair weld procedure that was developed was the result of past experiences of industry experts as well as trial and error in the field. Subsequent to the field work, laboratory investigations were performed in an attempt to understand metallurgical issues associated with weld cracking in this alloy. Key words: liquation cracking, niobium carbides, high temperature HAZ cracking, reformer outlet, high temperature castings
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 98443 REMAINING LIFE ASSESSMENT OF STEAM/
Available for download

98443 REMAINING LIFE ASSESSMENT OF STEAM/METHANE AND HYDROGEN REFORMER FURNACE TUBES

Product Number: 51300-98443-SG
ISBN: 98443 1998 CP
Author: Gordon P. Kallenberg
$20.00
Picture for 00512 HIGH TEMPERATURE AGING CHARACTERISTICS
Available for download

00512 HIGH TEMPERATURE AGING CHARACTERISTICS OF 20Cr32Ni1Nb CASTINGS

Product Number: 51300-00512-SG
ISBN: 00512 2000 CP
Author: J. J. Hoffman
$20.00