The stress corrosion crack growth rate was evaluated on controlled chemistries of Alloy 182 and Alloy 82 weld metals in 288° C BWR water. Variables included the effects of the composition/stabilization, stress intensity factor, dK/da, corrosion potential and water purity. In general, Alloy 82 weld metal only showed a ~2X lower growth rate than Alloy 182 weld metal. All materials showed a dependence on stress intensity factor of ~K2.2, consistent with other materials. Very strong effects of +dK/da (~100 – 1000X) were observed, but essentially no effect of –dK/da, compared to constant K data. Strong effects (~10X) of corrosion potential were observed, and relatively limited effects (~2X) of 0 – 30 ppb sulfate were observed.

Keywords: Stress corrosion cracking, nickel alloy weld metals, high temperature water, water chemistry, Alloy 182 weld metal, Alloy 82 weld metal, stress intensity factor
The stress corrosion crack growth rate was evaluated on controlled chemistries of Alloy 182 and Alloy 82 weld metals in 288° C BWR water. Variables included the effects of the composition/stabilization, stress intensity factor, dK/da, corrosion potential and water purity. In general, Alloy 82 weld metal only showed a ~2X lower growth rate than Alloy 182 weld metal. All materials showed a dependence on stress intensity factor of ~K2.2, consistent with other materials. Very strong effects of +dK/da (~100 – 1000X) were observed, but essentially no effect of –dK/da, compared to constant K data. Strong effects (~10X) of corrosion potential were observed, and relatively limited effects (~2X) of 0 – 30 ppb sulfate were observed.

Keywords: Stress corrosion cracking, nickel alloy weld metals, high temperature water, water chemistry, Alloy 182 weld metal, Alloy 82 weld metal, stress intensity factor
Product tags
Also Purchased
Picture for 10289 Effect of Severe Cold Work on the Microstructure and SSC Resistance of Superduplex SS
Available for download

10289 Effect of Severe Cold Work on the Microstructure and SSC Resistance of Superduplex Stainless Steel Downhold Tubulars

Product Number: 51300-10289-SG
ISBN: 10289 2010 CP
Author: Andrew J. Leonard, John W. Martin, Al P. Davis, Masakatsu Ueda and Shigemitsu Kimura
Publication Date: 2010
$20.00
Picture for 10280 HIC Performance of Heavy Wall Large-Diameter Pipes for Sour-Service Applications
Available for download

10280 HIC Performance of Heavy Wall Large-Diameter Pipes for Sour-Service Applications Under Fit-for-Service Conditions

Product Number: 51300-10280-SG
ISBN: 10280 2010 CP
Author: Thomas Haase, Christoph Bosch, Andreas Liessem and Jens Schroeder
Publication Date: 2010
$20.00
Picture for 10288 Environment Induced Cracking of Advanced Steam Turbine Blade Steels
Available for download

10288 Environment Induced Cracking of Advanced Steam Turbine Blade Steels

Product Number: 51300-10288-SG
ISBN: 10288 2010 CP
Author: A Turnbull and S Zhou