Soil seasonal change is believed to be one of the major factors that contribute to pipeline high pH stress corrosion cracking (SCC), although the specific role and mechanisms of the soil seasonal change in the pipeline high pH SCC susceptibility are not clearly understood. This study is aimed at investigating this role and the mechanisms of the soil seasonal change through mathematical modeling. The temporal and spatial variation, with soil seasonal change, of the solution chemistry and the pipe steel potential and corrosion rate in a coating disbonded region is explored. With the pipe potential at the holiday varied by soil seasonal wet and dry cycles, the model results suggest that the susceptible conditions of high pH SCC could be formed during soil wet seasons and seasonal transitions. Depending on the level of drought and the effectiveness of cathodic protection (CP) during dry seasons, the susceptible conditions of the pipe high pH SCC may or may not be possible to form.

Keywords: stress corrosion cracking, pipeline, cathodic protection, seasonal change, modeling
Soil seasonal change is believed to be one of the major factors that contribute to pipeline high pH stress corrosion cracking (SCC), although the specific role and mechanisms of the soil seasonal change in the pipeline high pH SCC susceptibility are not clearly understood. This study is aimed at investigating this role and the mechanisms of the soil seasonal change through mathematical modeling. The temporal and spatial variation, with soil seasonal change, of the solution chemistry and the pipe steel potential and corrosion rate in a coating disbonded region is explored. With the pipe potential at the holiday varied by soil seasonal wet and dry cycles, the model results suggest that the susceptible conditions of high pH SCC could be formed during soil wet seasons and seasonal transitions. Depending on the level of drought and the effectiveness of cathodic protection (CP) during dry seasons, the susceptible conditions of the pipe high pH SCC may or may not be possible to form.

Keywords: stress corrosion cracking, pipeline, cathodic protection, seasonal change, modeling
Product tags
Also Purchased
Picture for 08129 Overall Mechanisms of High pH and Near-Neutral pH SCC, Models for Forecasting SCC Susceptible
Available for download
Picture for 00362 GENERATION OF NEAR NEUTRAL pH AND HIGH
Available for download

00362 GENERATION OF NEAR NEUTRAL pH AND HIGH pH SCC ENVIRONMENTS ON BURIED PIPELINES

Product Number: 51300-00362-SG
ISBN: 00362 2000 CP
Author: K. Krist, R. R. Fessler, T. R. Jack and B. Erno
$20.00
Picture for 01211 EFFECT OF MICROSTRUCTURE AND MICROCHEMISTRY
Available for download

01211 EFFECT OF MICROSTRUCTURE AND MICROCHEMISTRY ON THE SCC BEHAVIOR OF ARCHIVAL AND MODERN PIPELINE STEELS IN A HIGH pH ENVIRONMENT

Product Number: 51300-01211-SG
ISBN: 01211 2001 CP
Author: Phil Dusek, Mike J. Danielson and Russell H. Jones
$20.00