09080 Case-History of Environmental Cracking Failures with Alloy K-500 for Downhole Completion Tools

Product Number: 51300-09080-SG
ISBN: 09080 2009 CP
Author: Greg B. Chitwood,Joshua Rooker and Karthik Krishnan
Publication Date: 2009
$0.00
$20.00
$20.00
Alloy K-500 saw widespread use as a high strength material for sour service in the oil field up to the mid-1980s. Its use declined after that, however, following field failures that were published in the literature of wellhead stems, subsea bolts, and drill stem tools. These failures appear to be unrelated to sour service. In the authors’ company, unpublicized failures of downhole tools made from Alloy K-500 were observed in sour service, causing the company to abandon Alloy K-500 for downhole tools in favor of other nickel alloys. As evidenced by the ballot to the NACE/ISO Maintenance Panel to extend the performance limits of Alloy K-500 in NACE MR0175 / ISO 15156-3A, it is obvious that there has been renewed interest by the industry in Alloy K-500. This ballot was based upon laboratory testing, and two attempts at passing the ballot failed. Committee discussion during the balloting suggested there was insufficient detail in the past field experience to compare directly with the laboratory data, and questions were also raised concerning the melt practice and metallurgical condition of the material that had failed in the field. These issues prompted the authors to conduct a historical review of their company’s past failures with the alloy. This paper will present three case histories from the early 1980's where Alloy K-500 experienced failures in downhole equipment. The intent of the paper is to put forward the field conditions under which the failures were seen and report the analysis done on the failed components. This could help the reader better understand the issues facing the use of Alloy K-500 alloy for downhole completion tools and shed additional light on the Maintenance Panel’s decision to reject a ballot for extended limits in NACE MR0175 / ISO 15156-3.
Alloy K-500 saw widespread use as a high strength material for sour service in the oil field up to the mid-1980s. Its use declined after that, however, following field failures that were published in the literature of wellhead stems, subsea bolts, and drill stem tools. These failures appear to be unrelated to sour service. In the authors’ company, unpublicized failures of downhole tools made from Alloy K-500 were observed in sour service, causing the company to abandon Alloy K-500 for downhole tools in favor of other nickel alloys. As evidenced by the ballot to the NACE/ISO Maintenance Panel to extend the performance limits of Alloy K-500 in NACE MR0175 / ISO 15156-3A, it is obvious that there has been renewed interest by the industry in Alloy K-500. This ballot was based upon laboratory testing, and two attempts at passing the ballot failed. Committee discussion during the balloting suggested there was insufficient detail in the past field experience to compare directly with the laboratory data, and questions were also raised concerning the melt practice and metallurgical condition of the material that had failed in the field. These issues prompted the authors to conduct a historical review of their company’s past failures with the alloy. This paper will present three case histories from the early 1980's where Alloy K-500 experienced failures in downhole equipment. The intent of the paper is to put forward the field conditions under which the failures were seen and report the analysis done on the failed components. This could help the reader better understand the issues facing the use of Alloy K-500 alloy for downhole completion tools and shed additional light on the Maintenance Panel’s decision to reject a ballot for extended limits in NACE MR0175 / ISO 15156-3.
Product tags
Also Purchased
Picture for 09028 Coatings Failures in Plants and Industrial Environment
Available for download

09028 Coatings Failures in Plants and Industrial Environment

Product Number: 51300-09028-SG
ISBN: 09028 2009 CP
Author: Mohammed Al-Sonidah and Oluwatoyin A. Ashiru
Publication Date: 2009
$20.00
Picture for 99633 COMPARISON OF HYDROGEN TRAPPING/TENSILE
Available for download

99633 COMPARISON OF HYDROGEN TRAPPING/TENSILE TESTING CORRELATIONS WITH FIELD SERVICE RESULTS FOR ALLOY K-500

Product Number: 51300-99633-SG
ISBN: 99633 1999 CP
Author: B. G. Pound
$20.00
Picture for 09083 Application Limits for 110ksi Strength Grade Super 13Cr Steel in CO2 Environments Containing S
Available for download

09083 Application Limits for 110ksi Strength Grade Super 13Cr Steel in CO2 Environments Containing Small Amounts of H2S

Product Number: 51300-09083-SG
ISBN: 09083 2009 CP
Author: Hideki Takabe, Perry Ian Nice, John W. Martin and Masakatsu Ueda
Publication Date: 2009
$20.00