07130 Investigating the Impact of Environment on Transgranular Stress Corrosion Cracking of Pipeline Steels

Product Number: 51300-07130-SG
ISBN: 07130 2007 CP
Author: Stefanie Asher and Preet Mohinder Singh
Publication Date: 2007
$0.00
$20.00
$20.00
Transgranular stress corrosion cracking (TGSCC) of buried carbon steel fuel transmission pipelines has been reported to occur on pipelines that are protectively coated and subjected to cathodic protection. The objective of this research was to investigate the conditions under which near-neutral pH environments can be formed. Specifically, this research focuses on how the pH of solutions change with applied potential and CO2 exposure. Potentiodynamic polarization tests were performed in solutions with different ground water constituents to see their role in anodic and cathodic behavior of pipeline steels. Application of cathodic protection alters the pH at the steel surface, shifting the environment outside of near-neutral pH conditions. Coupon exposure tests and potentiodynamic results suggest that the environment of TGSCC is possible in a wide range of temperatures and compositions.
Transgranular stress corrosion cracking (TGSCC) of buried carbon steel fuel transmission pipelines has been reported to occur on pipelines that are protectively coated and subjected to cathodic protection. The objective of this research was to investigate the conditions under which near-neutral pH environments can be formed. Specifically, this research focuses on how the pH of solutions change with applied potential and CO2 exposure. Potentiodynamic polarization tests were performed in solutions with different ground water constituents to see their role in anodic and cathodic behavior of pipeline steels. Application of cathodic protection alters the pH at the steel surface, shifting the environment outside of near-neutral pH conditions. Coupon exposure tests and potentiodynamic results suggest that the environment of TGSCC is possible in a wide range of temperatures and compositions.
Product tags
Also Purchased
Picture for 00370 RESEARCH CHALLENGES REGARDING STRESS
Available for download

00370 RESEARCH CHALLENGES REGARDING STRESS-CORROSION CRACKING OF PIPELINES

Product Number: 51300-00370-SG
ISBN: 00370 2000 CP
Author: R. R. Fessler, K. Krist
$20.00
Picture for 00363 A REVIEW OF STRESS CORROSION CRACKING OF
Available for download

00363 A REVIEW OF STRESS CORROSION CRACKING OF HIGH PRESSURE GAS PIPELINES

Product Number: 51300-00363-SG
ISBN: 00636 2000 CP
Author: R.N.Parkins
$20.00
Picture for 06175 Stress Corrosion Cracking of Pipeline Steel
Available for download

06175 Stress Corrosion Cracking of Pipeline Steel in Near-Neutral pH Environments

Product Number: 51300-06175-SG
ISBN: 06175 2006 CP
Author: Stefanie L. Asher, Jeffery A. Colwell, Preet M. Singh, Brian N. Leis
$20.00