07096 Effect of Variation of Local pH on Stress Corrosion Cracking of Stainless Steels in High Concentration Brines

Product Number: 51300-07096-SG
ISBN: 07096 2007 CP
Author: Hisashi Amaya, Masakatsu Ueda, Masayuki Sagara, and Kazuhiko Noda
Publication Date: 2007
$0.00
$20.00
$20.00
Recently, high density clear brine has been utilized in the oil and gas exploration field as completion or packer fluid in the annulus between the production casing and tubing. CaCl2 has been widely applied for the clear brine, however, some failure cases of duplex stainless steels or super martensitic stainless steels in high density CaCl2 brine have been reported. The effects of oxygen and/or production gas (CO2/H2S) contamination, or H2S formation as decomposition products of NaSCN-type inhibitor have been discussed. In this study, pH in high concentration brines was evaluated to discuss SCC susceptibility of stainless steels. Especially, the stability of pH in high concentration brines has been closely studied for the fundamental aspect to determine the effect of the variation of local pH on SCC behavior. pH imaging sensor (Scanning Chemical Microscope - SCHEM which can measure the two-dimensional pH distribution) was applied to examine the local pH distribution in high concentration brines. SCC susceptibilities of martensitic stainless steels and duplex stainless steels were evaluated in the combination of various brine concentrations and temperature conditions. The addition of caustic soda to high concentration CaCl2 brine made it stable at higher pH, and also reduced the SCC susceptibility. SCC susceptibility seems to depend on the stability of passive film. Therefore, the depassivation pH is considered to be the important factor affecting SCC in high concentration brines.
Recently, high density clear brine has been utilized in the oil and gas exploration field as completion or packer fluid in the annulus between the production casing and tubing. CaCl2 has been widely applied for the clear brine, however, some failure cases of duplex stainless steels or super martensitic stainless steels in high density CaCl2 brine have been reported. The effects of oxygen and/or production gas (CO2/H2S) contamination, or H2S formation as decomposition products of NaSCN-type inhibitor have been discussed. In this study, pH in high concentration brines was evaluated to discuss SCC susceptibility of stainless steels. Especially, the stability of pH in high concentration brines has been closely studied for the fundamental aspect to determine the effect of the variation of local pH on SCC behavior. pH imaging sensor (Scanning Chemical Microscope - SCHEM which can measure the two-dimensional pH distribution) was applied to examine the local pH distribution in high concentration brines. SCC susceptibilities of martensitic stainless steels and duplex stainless steels were evaluated in the combination of various brine concentrations and temperature conditions. The addition of caustic soda to high concentration CaCl2 brine made it stable at higher pH, and also reduced the SCC susceptibility. SCC susceptibility seems to depend on the stability of passive film. Therefore, the depassivation pH is considered to be the important factor affecting SCC in high concentration brines.
Product tags
Also Purchased
Picture for 07091 Effect of Alloying Element on Intergranular Stress Corrosion Cracking Susceptibility of Super
Available for download

07091 Effect of Alloying Element on Intergranular Stress Corrosion Cracking Susceptibility of Super Martensitic Stainless Steel Welded Joints in Sweet Environment

Product Number: 51300-07091-SG
ISBN: 07091 2007 CP
Author: Hisashi Amaya, Kazuhiro Ogawa, Akira Taniyama, and Masakatsu Ueda
Publication Date: 2007
$20.00
Picture for 07097 New Insights into the Potential for Environmental Cracking of Corrosion Resistant Alloys in Hi
Available for download

07097 New Insights into the Potential for Environmental Cracking of Corrosion Resistant Alloys in High-Density Formate and Bromide Well Completion Brines at High Temperature

Product Number: 51300-07097-SG
ISBN: 07097 2007 CP
Author: John D. Downs, Siv Howard, Mike Harris, William Benton, M. Billingham
Publication Date: 2007
$20.00
Picture for 05458 Effect of pH and Activity Coefficient of
Available for download

05458 Effect of pH and Activity Coefficient of Proton in High Concentration Brines on Stress Corrosion Cracking of Stainless Steels

Product Number: 51300-05458-SG
ISBN: 05458 2005 CP
Author: Hisashi Amaya, Takeo Kudo, Masakatsu Ueda, and Masayuki Sagara, Sumitomo Metal Industries Ltd.; Kazu
$20.00