02535 SUSCEPTIBILITY OF ALLOY 22 TO ENVIRONMENTALLY ASSISTED CRACKING IN YUCCA MOUNTAIN RELEVANT ENVIRONMENTS

Product Number: 51300-02535-SG
ISBN: 02535 2002 CP
Author: John C. Estill, Kenneth J. King, David V. Fix, Darryl G. Spurlock, Gary A. Hust, Steven R. Gordon, R
$0.00
$20.00
$20.00
In its current design, the high-level nuclear waste containers will include an external layer of Alloy 22 (Ni-22Cr-13Mo-3W-3Fe). Since over their life-time the containers may be exposed to multi-ionic aqueous environments, a potential degradation mode of the outer layer could be environmental assisted cracking (EAC). The objective of the current research work was to quantify the susceptibility of Alloy 22 to EAC in several environmental conditions including solution composition, temperature and electrochemical potential. The susceptibility to EAC was evaluated using the constant deformation technique, the compact tension specimen-low cycle fatigue method and the slow strain rate test (SSRT). The alloy was tested in the wrought mill annealed (MA) and in the as-welded conditions. Results show that Alloy 22 was extremely resistant to EAC in a wide range of environmental conditions. Using SSRT, Alloy 22 was found susceptible to EAC in one electrolyte at one temperature and at one electrochemical potential. Keywords: high-level nuclear waste, nickel-based alloy, N06022, environmentally assisted cracking, U-bend, slow strain rate test, compact specimens, crack propagation rate, simulated acidified water (SAW), simulated concentrated water (SCW), basic saturated water (BSW), simulated saturated water (SSW).
In its current design, the high-level nuclear waste containers will include an external layer of Alloy 22 (Ni-22Cr-13Mo-3W-3Fe). Since over their life-time the containers may be exposed to multi-ionic aqueous environments, a potential degradation mode of the outer layer could be environmental assisted cracking (EAC). The objective of the current research work was to quantify the susceptibility of Alloy 22 to EAC in several environmental conditions including solution composition, temperature and electrochemical potential. The susceptibility to EAC was evaluated using the constant deformation technique, the compact tension specimen-low cycle fatigue method and the slow strain rate test (SSRT). The alloy was tested in the wrought mill annealed (MA) and in the as-welded conditions. Results show that Alloy 22 was extremely resistant to EAC in a wide range of environmental conditions. Using SSRT, Alloy 22 was found susceptible to EAC in one electrolyte at one temperature and at one electrochemical potential. Keywords: high-level nuclear waste, nickel-based alloy, N06022, environmentally assisted cracking, U-bend, slow strain rate test, compact specimens, crack propagation rate, simulated acidified water (SAW), simulated concentrated water (SCW), basic saturated water (BSW), simulated saturated water (SSW).
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 00181 INFLUENCE OF AGING ON MICROSTRUCTURE
Available for download

00181 INFLUENCE OF AGING ON MICROSTRUCTURE, MECHANICAL PROPERTIES, AND CORROSION RESISTANCE OF A Ni-22Cr-13Mo-3W ALLOY.

Product Number: 51300-00181-SG
ISBN: 00181 2000 CP
Author: Rau1 B. Rebak, Natalie E. Koon, Jeffrey R. Dillman and Paul Crook, Tammy S. E. Summers
$20.00
Picture for 02542 EFFECT OF THERMAL AGING ON THE...
Available for download

02542 EFFECT OF THERMAL AGING ON THE CORROSION BEHAVIOR OF WROUGHT AND WELDED ALLOY 22.

Product Number: 51300-02542-SG
ISBN: 02542 2002 CP
Author: Rafil B. Rebak, Tammy S. Edgecumbe Summers, Tiangan Lian, Ricardo M. Carranza, Jeffrey R. Dillman, T
$20.00
Picture for 00206 STRESS CORROSION CRACKING, PASSIVE, AND
Available for download

00206 STRESS CORROSION CRACKING, PASSIVE, AND LOCALIZED CORROSION OF ALLOY 22 HIGH-LEVEL RADIOACTIVE WASTE CONTAINERS

Product Number: 51300-00206-SG
ISBN: 00206 2000 CP
Author: D.S. Dunn, Y.-M. Pan, and G.A. Cragnolino
$20.00