02425 STRESS CORROSION CRACKING OF NICKEL-CHROMIUM-MOLYBDENUM ALLOYS IN CHLORIDE SOLUTIONS

Product Number: 51300-02425-SG
ISBN: 02425 2002 CP
Author: D.S. Dunn, Y.-M. Pan and G.A. Cragnolino
$0.00
$20.00
$20.00
The stress corrosion cracking (SCC) susceptibilities of Alloy 22 and Type 316L stainless steel were evaluated in concentrated chloride solutions. Test results indicate that Alloy 22 is very resistant to chloride SCC. No SCC was observed after 12 months in 14.0 molal... Keywords: Stress corrosion cracking, localized corrosion, stainless steel, nickel base alloys, nuclear waste disposal
The stress corrosion cracking (SCC) susceptibilities of Alloy 22 and Type 316L stainless steel were evaluated in concentrated chloride solutions. Test results indicate that Alloy 22 is very resistant to chloride SCC. No SCC was observed after 12 months in 14.0 molal... Keywords: Stress corrosion cracking, localized corrosion, stainless steel, nickel base alloys, nuclear waste disposal
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 02423 CHLORIDE STRESS CORROSION CRACKING...
Available for download

02423 CHLORIDE STRESS CORROSION CRACKING RESISTANCE OF 6% Mo STAINLESS STEEL ALLOY

Product Number: 51300-02423-SG
ISBN: 02423 2002 CP
Author: Ronald. J. Gerlock and James D. Fritz
$20.00
Picture for 10287 Critical Stress Corrosion Cracking Potentials of Stainless Steels in Dilute Chloride Solutions
Available for download

10287 Critical Stress Corrosion Cracking Potentials of Stainless Steels in Dilute Chloride Solutions

Product Number: 51300-10287-SG
ISBN: 10287 2010 CP
Author: Janardhan Rao Saithala, Steve McCoy, John Atkinson and Harvindher Singh Ubhi
Publication Date: 2010
$20.00