Save 20% on select titles with code HIDDEN24 - Shop The Sale Now
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact AMPP Customer Support for assistance.
Error Message:
Please login to use Standards Credits*
* AMPP Members receive Standards Credits in order to redeem eligible Standards and Reports in the Store
You are not a Member.
AMPP Members enjoy many benefits, including Standards Credits which can be used to redeem eligible Standards and Reports in the Store.
You can visit the Membership Page to learn about the benefits of membership.
You have previously purchased this item.
Go to Downloadable Products in your AMPP Store profile to find this item.
You do not have sufficient Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your Standards Credit(s)
1
Remaining Credits
0
Please review your transaction.
Click on 'REDEEM' to use your Standards Credits to claim this item.
You have successfully redeemed:
Go to Downloadable Products in your AMPP Store Profile to find and download this item.
The investigation on the specimens in the SCC susceptible conditions is included in Part 1, AMPP conference paper C2022-179982. In this Part 2, a case study is presented on the local corrosion on specimen surface or shoulder area although high ductility ratios in two testing conditions.
Standards NACE(1) MR0175 / ISO(2) 15156-31 have temperature-H2S-Cl-pH limits for safely using duplex stainless steels based on their Pitting Resistance Equivalent Number (PREN) of subcategory such as duplex stainless steel (DSS, PREN 30-40, Mo>1.5%) and super duplex stainless steel (SDSS, PREN 4045), temperature-pH domain of stress corrosion cracking (SCC) resistance can be used for material evaluation and provided by using slow strain rate testing (SSRT) screening in sour testing conditions2.