Picture for Influence of Centerline Intermetallic Stringers on Pitting Corrosion Resistance of Superduplex Stainless Steels
Available for download

Influence of Centerline Intermetallic Stringers on Pitting Corrosion Resistance of Superduplex Stainless Steels

Product Number: 51321-16298-SG
Author: Paulina Erazmus-Vignal Sayens /Vincent Vignal/Pauline HUGUENIN/Florent KRAJCARZ/Clément BOISSY/Saghi SAEDLOU/Patrick Toussaint
Publication Date: 2021
$20.00