Complications occur in orthopedic surgery. Corrosion of magnesium W4 alloy was investigated in vitro by electrochemical methods in solutions replicating the body's environment. To control the biodegradation of titanium and magnesium implants, bio active PEO coatings are essential for biomedical implants.
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact AMPP Customer Support for assistance.
Error Message:
Please login to use Standards Credits*
* AMPP Members receive Standards Credits in order to redeem eligible Standards and Reports in the Store
You are not a Member.
AMPP Members enjoy many benefits, including Standards Credits which can be used to redeem eligible Standards and Reports in the Store.
You can visit the Membership Page to learn about the benefits of membership.
You have previously purchased this item.
Go to Downloadable Products in your AMPP Store profile to find this item.
You do not have sufficient Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your Standards Credit(s)
1
Remaining Credits
0
Please review your transaction.
Click on 'REDEEM' to use your Standards Credits to claim this item.
You have successfully redeemed:
Go to Downloadable Products in your AMPP Store Profile to find and download this item.
Industrial usage of Plasma Electrolytic Oxidation (PEO) has grown consistently in recent years, thanks to the improved characteristics imparted to the oxide film in terms of surface adhesion, hardness, crystallinity, uniformity, and corrosion resistance. The metallic substrate is not subjected to elevated temperature and the overall equipment complexity is relatively simple, making the technique a good candidate for surface functionalization. In PEO treatments, high voltages are employed (~ 150-750 V 1) allowing for the formation of an insulating, or at least semiconductive, oxide layer that’s limits ion transport responsible for the initial coating growth. Beyond the spark voltage (prerequisite the enter the PEO regime) oxidation does not occur only as the result of a continuous flow of ions but rather it takes place after the cooling of a plasma discharge.